🗣 SL提问: immersion gold
✍️ Ai批改: Immersion gold, also known as electroless nickel immersion gold (ENIG), is a widely used surface finish in the printed circuit board (PCB) industry、It involves depositing a thin layer of gold over a nickel layer on copper surfaces through a chemical process、Here's a breakdown of its key aspects:
1、Process Overview
Step 1: Cleaning
The PCB is cleaned to remove oxides and contaminants from the copper surface.
Step 2: Micro-Etching
A light etch (e.g., with sulfuric acid) roughens the copper to improve adhesion.
Step 3: Activation
Palladium catalyst is applied to activate the surface for nickel deposition.
Step 4: Electroless Nickel Plating
A chemical bath deposits a layer of nickel (typically 3–6 µm thick) onto the copper.
Step 5: Immersion Gold
A thin gold layer (0.05–0.2 µm) is deposited via a displacement reaction, replacing nickel atoms at the surface.
2、Key Advantages
Excellent Solderability: Gold ensures reliable solder joints, especially for fine-pitch components.
Oxidation Resistance: Protects underlying copper and nickel from corrosion.
Flat Surface: Ideal for ball grid arrays (BGAs) and chip-on-board (COB) applications.
Durability: Resists wear on contact fingers (e.g., in connectors).
Long Shelf Life: Maintains performance over time.
3、Applications
High-Reliability Electronics: Aerospace, medical devices, automotive systems.
High-Frequency Circuits: Gold’s conductivity is critical for RF and microwave PCBs.
Consumer Electronics: Smartphones, laptops, and wearables with fine-pitch components.
Connectors and Contact Points: Ensures stable electrical connections.
4、Pros and Cons
| Pros | Cons |
|
| Excellent solderability | Higher cost than HASL or OSP |
| Flat, uniform surface | Risk of tin whiskers if nickel is improperly processed |
| Long-term reliability | Requires strict process control (e.g., pH, bath concentration) |
| Compatible with lead-free soldering | Environmental concerns due to gold/nickel usage |
5、Comparison with Other Finishes
| Finish | ENIG | HASL | OSP | Immersion Tin |
-
| Cost | High | Low | Low | Medium |
| Solderability | Excellent | Good | Good | Good |
| Flatness | Very flat | Wavy | Flat | Flat |
| Durability | High | Moderate | Low | Moderate |
| Lead-Free Compatibility | Yes | Yes | Yes | Yes |
6、Common Issues
Black Pad Syndrome: Caused by improper nickel plating, leading to brittle solder joints.
Gold Thickness Variations: Too thick can cause brittleness; too thin may compromise protection.
Nickel Oxidation: If the nickel layer is not properly sealed, it can degrade over time.
7、Industry Trends
Environmental Regulations: Stricter rules on gold/nickel waste management.
Advanced ENIG Variants: Newer processes (e.g., EPIG electroless palladium immersion gold) aim to reduce costs and improve reliability.
Miniaturization: ENIG remains critical for high-density PCBs in 5G and IoT devices.
If you have a specific question about immersion gold (e.g., cost, design considerations, or alternatives), feel free to ask!
0
IP地址: 251.178.139.160
搜索次数: 34
提问时间: 2025-06-28 00:25:08
❓️ 热门提问:
2019黄金价格走势图
今日黄金现货多少钱一克
1974年属虎可以戴黄金吗
合生东郊开盘价
ai十传媒龙头股票
750黄金卖价格
外贸公司如何收外汇
前海开源北证50成份指数发起C
外贸网站优化多少钱
华宝积极配置三个月持有混合(FOF)
豌豆Ai站群搜索引擎系统
🤝 关于我们:
三乐Ai
作文批改
英语分析
在线翻译
拍照识图
Ai提问
英语培训
本站流量
联系我们
📢 温馨提示:本站所有问答由Ai自动创作,内容仅供参考,若有误差请用“联系”里面信息通知我们人工修改或删除。
👉 技术支持:本站由豌豆Ai提供技术支持,使用的最新版:《豌豆Ai站群搜索引擎系统 V.25.05.20》搭建本站。